Objective To evaluate the marginal microleakage of porcelain-fused-to-metal crown using four different cements. Methods Sixteen porcelain-fused-to-metal crowns were built and randomly divided into 4 group, luted onto standard prepared human forward molars using four different cements(glass ionomer cement, resin-modified glass ionomer cement, PanaviaF, Super-Bond C&B adhesive luting system). After temperature cycling test, all the crowns were then submerged in 2% fuchsin for 24 h. The marginal microleakage at tooth cement interfaces was observed using light stereomicroscopy and evaluated in classification index. The marginal microleakage grade of 4 groups were analyzed by SPSS 13.0. Results The PanaviaF demonstrated the least marginal microleakage, Super-Bond C&B adhesive luting system, resin-modified glass ionomer cement showed an intermediate level of marginal microleakage, glass ionomer cement was associated with severe marginal microleakage(total, 掊2=157.60, P